Topic: PLA speed?
I am experiencing roughly 48 hours per kg with PLA, it seems the pellets simply cannot feed fast enough into the filastruder as they can with ABS. All PLA pellets I have found are around 3-4mm round. Has anyone been able to speed up PLA?
I am extruding at 150C with the fan barely blowing on the plastic running at 6v to keep speed and CFM down.
ABS times are around 10 hours per kg, which I am extremely happy about. I find myself using PLA almost as fast as I can make it and I am only using a single printer at the moment. Any assistance is greatly appreciated!