1 (edited by cmaloney 2016-01-10 15:54:51)

Topic: Feed screw not long enough?

I'm not sure what the problem is, but the motor cant reach the end of the screw bit when the bearing is compressed and 5mm is sticking out the end of the pipe.  Any ideas?

http://soliforum.com/i/?cigsdmn.jpg
http://soliforum.com/i/?HQE1MB4.jpghttp://soliforum.com/i/?AsVHe4Y.jpg


Edit: Nevermind, Tim said I could just use a deep socket piece.  I'll try that, thanks!

2

Re: Feed screw not long enough?

I replied to your email with comments. smile