1 (edited by dubbsd 2016-01-01 13:54:24)

Topic: Why did this start air printing -UPDATED - JSON file included

as you can see from the photo a few layers into the print it started airprinting
I was using both extruders with HIPS in extruder 0
I ran the file through Netfab and it still done it.
I changed to do all with extruder 1 and it is working fine
http://soliforum.com/i/?xJnrGsd.jpg
http://soliforum.com/i/?6aMR0OL.jpg

Ultimaker S3.

2

Re: Why did this start air printing -UPDATED - JSON file included

Here is the Json file for the failed print.

{
   "version" : "3.8.0.168",
   "_bot" : "replicator2x",
   "_extruders" : [ 2 ],
   "_materials" : [ "abs", "hips" ],
   "description" : "raft & Support",
   "infillDensity" : 0.1000000014901161,
   "layerHeight" : 0.2000000029802322,
   "maxSparseFillThickness" : 0.2000000029802322,
   "numberOfShells" : 2,
   "shellsLeakyConnections" : false,
   "insetDistanceMultiplier" : 1.0,
   "infillShellSpacingMultiplier" : 0.70,
   "adjacentFillLeakyConnections" : false,
   "adjacentFillLeakyDistanceRatio" : 0,
   "maxConnectionLength" : 10.0,
   "roofThickness" : 0.8000000119209290,
   "floorThickness" : 0.8000000119209290,
   "roofAnchorMargin" : 0.40,
   "coarseness" : 9.999999747378752e-005,
   "gridSpacingMultiplier" : 1.0,
   "doExternalSpurs" : true,
   "doInternalSpurs" : false,
   "minSpurWidth" : 0.120,
   "maxSpurWidth" : 0.50,
   "minSpurLength" : 0.340,
   "spurOverlap" : 0.0010,
   "extruderTemp0" : 250,
   "extruderTemp1" : 230,
   "platformTemp" : 110,
   "travelSpeedXY" : 150.0,
   "travelSpeedZ" : 23.0,
   "doRaft" : true,
   "raftModelSpacing" : 0.3499999940395355,
   "raftOutset" : 4.0,
   "raftExtraOffset" : 0.0,
   "raftBaseLayers" : 1,
   "raftBaseThickness" : 0.3000000119209290,
   "raftBaseWidth" : 2.50,
   "raftBaseDensity" : 0.6999999880790710,
   "raftBaseAngle" : 0.0,
   "raftBaseRunLength" : 15.0,
   "raftBaseRunGapRatio" : 0.8000000119209290,
   "minRaftBaseGap" : 0.0,
   "raftInterfaceLayers" : 1,
   "raftInterfaceThickness" : 0.2700000107288361,
   "raftInterfaceWidth" : 0.4000000059604645,
   "raftInterfaceDensity" : 0.3000000119209290,
   "raftInterfaceAngle" : 45.0,
   "raftSurfaceLayers" : 2,
   "raftSurfaceThickness" : 0.2000000029802322,
   "raftSurfaceAngle" : 0.0,
   "raftSurfaceShells" : 2,
   "raftSurfaceShellSpacingMultiplier" : 0.70,
   "raftAligned" : true,
   "doBreakawaySupport" : true,
   "supportAngle" : 68.0,
   "supportRoofModelSpacing" : 0.4000000059604645,
   "supportModelSpacing" : 0.4000000059604645,
   "supportExtraDistance" : 0.50,
   "supportDensity" : 0.2000000029802322,
   "supportExcessive" : false,
   "supportAligned" : true,
   "supportLeakyConnections" : true,
   "doSupport" : false,
   "defaultSupportMaterial" : 0,
   "doMixedSupport" : false,
   "defaultRaftMaterial" : 0,
   "doMixedRaft" : false,
   "purgeWallModelOffset" : 2.0,
   "purgeWallSpacing" : 1.0,
   "purgeWallWidth" : 0.50,
   "purgeWallBasePatternWidth" : 8.0,
   "purgeWallBaseFilamentWidth" : 2.0,
   "purgeWallBasePatternLength" : 10.0,
   "purgeWallPatternWidth" : 2.0,
   "purgeBucketSide" : 4.0,
   "purgeWallXLength" : 30.0,
   "doPurgeWall" : true,
   "bedZOffset" : 0.0,
   "minLayerHeight" : 0.010,
   "startPosition" : {
      "x" : -112,
      "y" : -73.0,
      "z" : 0
   },
   "startGcode" : "",
   "endGcode" : "",
   "doPrintProgress" : true,
   "minLayerDuration" : 5.0,
   "doExponentialDeceleration" : false,
   "exponentialDecelerationMinSpeed" : 0.0,
   "defaultExtruder" : 0,
   "extruderProfiles" : [
      {
         "feedDiameter" : 1.769999980926514,
         "toolchangeRetractDistance" : 19.0,
         "toolchangeRetractRate" : 6.0,
         "toolchangeRestartDistance" : 18.50,
         "toolchangeRestartRate" : 6.0,
         "feedstockMultiplier" : 0.9300000000000001,
         "nozzleDiameter" : 0.40,
         "retractDistance" : 1.299999952316284,
         "retractRate" : 25.0,
         "retractDistance2" : 0,
         "retractRate2" : 50,
         "restartRate" : 25.0,
         "restartExtraDistance" : 0.0,
         "restartExtraDistance2" : 0,
         "restartExtraRate" : 25.0,
         "restartExtraRate2" : -1,
         "firstLayerExtrusionProfile" : "firstLayer",
         "firstLayerRaftExtrusionProfile" : "firstLayerRaft",
         "insetsExtrusionProfile" : "insets",
         "infillsExtrusionProfile" : "infill",
         "outlinesExtrusionProfile" : "outlines",
         "raftBaseExtrusionProfile" : "raftBase",
         "raftExtrusionProfile" : "raft",
         "bridgesExtrusionProfile" : "bridges"
      },
      {
         "feedDiameter" : 1.769999980926514,
         "toolchangeRetractDistance" : 19.0,
         "toolchangeRetractRate" : 6.0,
         "toolchangeRestartDistance" : 18.50,
         "toolchangeRestartRate" : 6.0,
         "feedstockMultiplier" : 0.9300000000000001,
         "nozzleDiameter" : 0.40,
         "retractDistance" : 1.299999952316284,
         "retractRate" : 25.0,
         "retractDistance2" : 0,
         "retractRate2" : 50,
         "restartRate" : 25.0,
         "restartExtraDistance" : 0.0,
         "restartExtraDistance2" : 0,
         "restartExtraRate" : 25.0,
         "restartExtraRate2" : -1,
         "firstLayerExtrusionProfile" : "firstLayer",
         "firstLayerRaftExtrusionProfile" : "firstLayerRaft",
         "insetsExtrusionProfile" : "insets",
         "infillsExtrusionProfile" : "infill",
         "outlinesExtrusionProfile" : "outlines",
         "raftBaseExtrusionProfile" : "raftBase",
         "raftExtrusionProfile" : "raft",
         "bridgesExtrusionProfile" : "bridges"
      }
   ],
   "extrusionProfiles" : {
      "firstLayer" : {
         "feedrate" : 30.0,
         "temperature_disabled" : 230.0
      },
      "firstLayerRaft" : {
         "feedrate" : 50.0,
         "temperature_disabled" : 230.0
      },
      "insets" : {
         "feedrate" : 90.0,
         "temperature_disabled" : 230.0
      },
      "infill" : {
         "feedrate" : 90.0,
         "temperature_disabled" : 230.0
      },
      "outlines" : {
         "feedrate" : 40.0,
         "temperature_disabled" : 230.0
      },
      "raftBase" : {
         "feedrate" : 10.0,
         "temperature_disabled" : 230.0
      },
      "raft" : {
         "feedrate" : 90.0,
         "temperature_disabled" : 230.0
      },
      "bridges" : {
         "feedrate" : 40.0,
         "temperature_disabled" : 230.0
      }
   },
   "backlashZ" : 0.0,
   "doBacklashCompensation" : false,
   "backlashX" : 0.0,
   "backlashY" : 0.090,
   "backlashFeedback" : 0.90,
   "backlashEpsilon" : 0.050,
   "doDynamicSpeed" : false,
   "dynamicSpeedDetectionWindow" : 3.0,
   "dynamicSpeedCurvatureThreshold" : 15,
   "dynamicSpeedSlowdownRatio" : 0.30,
   "doDynamicSpeedGradually" : true,
   "dynamicSpeedTransitionWindow" : 6.0,
   "dynamicSpeedTransitionShape" : 0.40,
   "doDynamicSpeedOutermostShell" : true,
   "doDynamicSpeedInteriorShells" : false,
   "doSplitLongMoves" : true,
   "splitMinimumDistance" : 0.40,
   "doBridging" : true,
   "doSupportUnderBridges" : false,
   "bridgeAnchorWidth" : 0.80,
   "bridgeAnchorMinimumLength" : 0.80,
   "bridgeMaximumLength" : 100.0,
   "bridgeSpacingMultiplier" : 1.0,
   "minSpeedMultiplier" : 0.30,
   "sparseInfillPattern" : "diamond (fast)",
   "commentOpen" : ";",
   "commentClose" : "",
   "roofLayerCount_disabled" : 4,
   "floorLayerCount_disabled" : 4,
   "infillOrientationOffset" : 0,
   "infillOrientationInterval" : 90,
   "infillOrientationRange" : 90,
   "solidFillOrientationOffset" : -45,
   "solidFillOrientationInterval" : 90,
   "solidFillOrientationRange" : 90,
   "anchorWidth" : 2.0,
   "anchorExtrusionAmount" : 5.0,
   "anchorExtrusionSpeed" : 2.0,
   "jsonToolpathOutput" : false,
   "metadataOutput" : false,
   "configPath" : "",
   "doFixedShellStart" : true,
   "fixedShellStartDirection" : 215.0,
   "floorLayerCount_disabled" : 4,
   "layerHeightMaximum" : 0.270,
   "layerHeightMinimum" : 0.120,
   "roofLayerCount_disabled" : 4
}
Here is the preview file.
http://soliforum.com/i/?s7rFTPa.jpg

Ultimaker S3.

3

Re: Why did this start air printing -UPDATED - JSON file included

hey dubbsd, 

I think your questions would get more traction in the general 3D Printer discussion forum, rather than the Solidoodle specific forums.

I doubt most of us familiar with the Solidoodle would know what a JASON file is, since it's not a common Solidoodle file format.  This is the equivalent of the pre-amble in the STL files that are output by Slic3r or Cura. 

But not being familiar with MakerBot I can't help you

To print or, 3D print, that is the question...
SD3 printer w/too many mods,  Printrbot Simple Maker Ed.,  FormLabs Form 1+
AnyCubic Photon, Shining 3D EinScan-S & Atlas 3D scanners...
...and too much time on my hands.

4

Re: Why did this start air printing -UPDATED - JSON file included

Thanks pirvin
I sent wardjr a PM and asked him to move it.

Ultimaker S3.