Topic: DaVinci Jr - Some noob questions
Hi everybody,
Like many folks Santa brought me a DaVinci Jr (well at $224 I had to have it!)
Took some fiddling, but have it printing now.
I have a couple of questions I am hoping somebody more experienced can provide some guidance on
1) Bed Tape - I have been using the ones that come with the printer but they tear pretty easy. I have seen suggestions of using masking tape or blue painters tape - any advice here? Also how do you put it on, simply in strips, or is there something more complicated?
2) Removing objects. So my printed objects are REALLY difficult to get off - to the point I damage them slightly trying to pry them from the bed - I am also worried that putting this much pressure on the bed will move it so it doesn't print correctly. And advice here on how to get the objects off easily?
3) Optimal settings. My printer came with a z-offset of 1.3mm - this seems to be ok and I haven't messed with it (yet!). In the XYZ software I export with a setting of 200 microns which seems to give reasonable results - I can push it to 100 which would give great results but I suspect take a lot of time!!! Any advice on what settings are best or just experiment and see?
4) Software. So I will be looking to design some of my own objects soon and wanted to find out the best software. I am NOT an artist (actually a software engineer by trade). So I think OpenSCAD is my best bet given I am very comfortable writing code to create the objects. Thoughts on that choice?
Any help is very much appreciated
Thanks
Simon