Topic: XYZ Duo with Repetier and KISSlicer - Help!
Hello there -
I am looking for a hand in using KISSlicer with my XYZ duo. I recently hacked my XYZ and dropped Repetier 0.92 FW in and am using Repetier Host to print. I have used Slic3r with great results on simple models but find that it freezes rather horribly on complex surfaces (>72 hours processing with no result on this model). I am printing ABS with HIPS support.
So, I took my model into KISSlicer and did my best based on available tuts and docs and got a great result in KISS in less than a minute. I was stoked so I purchased the PRO version to support my dual extruders. When I take my exported GCODE to Reptier I end up with something totally unexpected. The slice seems to be totally destroyed as a result (see attached image).
I know I am missing some settings in KISS but can you all help with some pointed suggestions?
Many Thanks!