1

Topic: Workbench and Simplify3d

hi hope you can help; i have a workbench and tryting to use simplify 3D, the main issue is the first layer, I run the G29 code (for auto probing) but i dont know if the software calculates the offset properly,the first layer seems to be not properly squished to the bed (higher)is there anyother code to do so? do I need to change any offset (m851)any help will be appreciate it  thanks.

2

Re: Workbench and Simplify3d

userksh14 wrote:

hi hope you can help; i have a workbench and tryting to use simplify 3D, the main issue is the first layer, I run the G29 code (for auto probing) but i dont know if the software calculates the offset properly,the first layer seems to be not properly squished to the bed (higher)is there anyother code to do so? do I need to change any offset (m851)any help will be appreciate it  thanks.


Just manually adjust the bed levelers as the print starts so you get the proper squish. Once you do that it should stay the same for all prints.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3 (edited by userksh14 2015-10-27 22:44:22)

Re: Workbench and Simplify3d

Thanks I´ll try, just one concern,  the software will compensate that everytime the printer measures?

4

Re: Workbench and Simplify3d

userksh14 wrote:

Thanks I´ll try, just one concern,  the software will compensate that everytime the printer measures?


The printer won't measure unless you send a G92 command or you have the command in your start gcode. Just comment it out of your start gcode and don't send the command manually.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

5

Re: Workbench and Simplify3d

got it, thanks a lot