Update:
Wow! The quality I got after purging and installing the melt filter/nozzle is amazing. The color is true with a 2/3% mixture by volume and extrudes in my printer setup better than Octave filament. I took a side by side pic and nobody guessed right.....even with a worn nozzle and significant bed sway...even my wife approved! ![]()
I will add pics, but I'm wondering why I lost diameter consistency. After purging the MG94, I began a few runs with PA747 and then quality went from .02 +/- to .05+/- even after upping temps to 187c as Revolve3D mentioned in the DIY threads. Exact temp was not mentioned, but higher than in the Filastruder .pdf
I still stand by the Filastruder purchase and recommend it to others. Talk about self-sufficiency!