Topic: Cura Made The Bed Crash
The dual 190mm high(Davinci 1.0 max is 200mm) 12hr print had just finished when I came in.
Just as the print ended, up went the bed as the extruder marched over on its X axis.
The bed stopped while the steppers were grinding away. The part jammed underneath the extruder.
Quick hit the off button and wedged out the pieces.
Heres was the end code in Cura:
; Default end code
G1 X0 Y0 Z130 ; Get extruder out of way Yeah-right!
M107 ; Turn off fan
; Disable all extruder
G91 ; Relative positioning
{IF_EXT0}T0
{IF_EXT0}G1 E-1 ; Reduce filament pressure
M104 T0 S0
G90 ; Absolute positioning
G92 E0 ; Reset extruder position
M140 S0 ; Disable heated bed
M84 ; Turn steppers off
What I replaced afterwards:
; Default end code
G91 Z10 F200 ; lower bed 10 relative to print
G28 X0 Y0 ; home
M107 ; Turn off fan
; Disable all extruder
G91 ; Relative positioning
{IF_EXT0}T0
{IF_EXT0}G1 E-1 ; Reduce filament pressure
M104 T0 S0
G90 ; Absolute positioning
G92 E0 ; Reset extruder position
M140 S0 ; Disable heated bed
M84 ; Turn steppers off
Repetier FW 0.92, Solidify3D