Topic: Upgraded glass bed (Intresting)
Ok after a lot of arguing with XYZ they agreed to post me a replacement glass bed. However while I'm waiting for it to arrive I spotted upgraded ones online , so I ordered Two spares. They arrived today
except royal mail stung me with a £8 customs handling fee and £14 in tax. Anyway it looks interesting. The heater looks much better covering all corners of the bed. Don't know when I will get chance to install it as I'm away for a week or so but cant wait to give it a try
Info says
DaVinci Zone Borosilicate glass Heated Bed for the DaVinci 1.0 3D printer
Replace the broken or chipped heated bed on your XYZPrinting's Da Vinci model 3D printer.
Simple installation as it is the same size, voltage and wire length as the original.
Improved heater design for more consistent heating
Genuine Borofloat glass for long, warp free life
Will not fit the Da Vinci Duo 3D printer.
Product Description:
Borosilicate glass with heater attached for the XYZPrinting Da Vinci 1.0 3D Printer.
Direct replacement for the original heater / glass unit.
Superior Borosilicate glass withstands heating without warping.
Specifications:
Borosilicate glass (Borofloat brand)
210 x 210 x 3.3mm glass size
12v 140watt heater from original equipment manufacturer.
Heater attached to glass in the same manner as the original.
Plug and play installation:
1. Disconnect the two electric connections
2. Unscrew the 4 screws for the original heated bed
3. Remove the old unit
4. Install the Borosilicate glass heater
5. Install the 4 screws
6. Connect the two electric connections
7. Calibrate the printer