1 (edited by DopeSkrit 2015-10-07 19:19:04)

Topic: Prints shifted Z Axis / Can some one diagnose it?

Hello something deleted all of my Slic3r Profiles and I had to start configuring my Slic3r again now i am getting a Z-Shift. I've fixed my bed it isnt wiggeling arround. (All set to 40mm/s)

Post's attachments

IMG_0708.JPG
IMG_0708.JPG 1.89 mb, file has never been downloaded. 

repetier.JPG
repetier.JPG 50.84 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
Da Vinci 1.0A Blue | Codename: FreeVinci | E3D v6 Bowden Custom Carriage | Printing PLA, ABS and PETG using S3D
Fabrikator Mini Orange | Printing PLA using Cura
Only printing with sub 20 Euro filaments.

2

Re: Prints shifted Z Axis / Can some one diagnose it?

does it get worse and worse the farther up you get?  Since the cross section of that model is reducing as you move up it almost looks like your running too hot or something, i get that sometimes on smaller tall things, the models themselves will move around because they are too soft and you get that.

3

Re: Prints shifted Z Axis / Can some one diagnose it?

Could be your glass bed moving or z axis wobble.

4 (edited by DopeSkrit 2015-10-07 19:00:53)

Re: Prints shifted Z Axis / Can some one diagnose it?

FrozenRC wrote:

Could be your glass bed moving or z axis wobble.

That dont fixed the issue.

Da Vinci 1.0A Blue | Codename: FreeVinci | E3D v6 Bowden Custom Carriage | Printing PLA, ABS and PETG using S3D
Fabrikator Mini Orange | Printing PLA using Cura
Only printing with sub 20 Euro filaments.

5

Re: Prints shifted Z Axis / Can some one diagnose it?

batmaster wrote:

does it get worse and worse the farther up you get?  Since the cross section of that model is reducing as you move up it almost looks like your running too hot or something, i get that sometimes on smaller tall things, the models themselves will move around because they are too soft and you get that.

Yes it does.

Da Vinci 1.0A Blue | Codename: FreeVinci | E3D v6 Bowden Custom Carriage | Printing PLA, ABS and PETG using S3D
Fabrikator Mini Orange | Printing PLA using Cura
Only printing with sub 20 Euro filaments.