Topic: New RH settings with solidoodle 3 / E3d V6
So I finally have everything up and running again with successful prints after many issues one leading into another, now I'm just curious as to the correct settings and calibrations in RH and slic3r. For some reason after a print finishes, my bed drops some, which i told it to do, but my print head will shift from the home spot in the back corner to the opposite corner and keep going a little too much causing a grinding noise to pop up and i can't imagine thats good for it. Also, my prints are smooth but kinda wavy in a way. The waves on it are very uniform and go up the layers in sort of a diagonal fashion. This only occurs on the shorter lengths of the perimeters whereas the longer lengths are pretty much perfect. I have my extrusion and flow rate perfectly calibrated so i know thats not it. Btw thank you to all who have helped me along the way in getting my printer fixed, you guys are awesome!