Topic: post repetier question
How often you guys level the bed? mine was fine fr about a week and today E3d V6, clicking... re-leveled the bed and all fine, just curious...
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → post repetier question
How often you guys level the bed? mine was fine fr about a week and today E3d V6, clicking... re-leveled the bed and all fine, just curious...
How often you guys level the bed? mine was fine fr about a week and today E3d V6, clicking... re-leveled the bed and all fine, just curious...
Depends on how rough you need to get to remove a print. If they pop right off like they should when cool then rarely, maybe once a month. If you are rough could be weekly or after each job.
How often you guys level the bed? mine was fine fr about a week and today E3d V6, clicking... re-leveled the bed and all fine, just curious...
Depends on how rough you need to get to remove a print. If they pop right off like they should when cool then rarely, maybe once a month. If you are rough could be weekly or after each job.
Depends on how rough you need to get to remove a print. If they pop right off like they should when cool then rarely, maybe once a month. If you are rough could be weekly or after each job.
What is the relationship between (good) bed level and roughness to remove prints?
carl_m1968 wrote:Depends on how rough you need to get to remove a print. If they pop right off like they should when cool then rarely, maybe once a month. If you are rough could be weekly or after each job.
What is the relationship between (good) bed level and roughness to remove prints?
The design of the adjusters is very bad and can be knocked out of adjustment simply by removing a part.
Antonious wrote:What is the relationship between (good) bed level and roughness to remove prints?
The design of the adjusters is very bad and can be knocked out of adjustment simply by removing a part.
Wonderful! When I'm "attacking" the bed to peel off the print I think about the risk for decalibration. You support my suspicion.