Topic: Extruding PVA?

Has anyone had any luck with this? I remember hearing that PVA supposedly decomposes into some nasty stuff when it gets too hot, so obviously that could be problematic.

2

Re: Extruding PVA?

Where'd you see that avoid thermal decomposition? Here's the MSDS for Esun PVA:

https://cdn.shopify.com/s/files/1/0389/ … 4.pdf?7844

I have a writeup someone sent me on their PVA success, if you're interested I can upload it. As usual, a big key is pre drying the polymer.

3

Re: Extruding PVA?

elmoret wrote:

Where'd you see that avoid thermal decomposition? Here's the MSDS for Esun PVA:

https://cdn.shopify.com/s/files/1/0389/ … 4.pdf?7844

I have a writeup someone sent me on their PVA success, if you're interested I can upload it. As usual, a big key is pre drying the polymer.

They killed your link. It only takes you to their frontend.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

4

Re: Extruding PVA?

Bummer. You can go here:

http://www.toybuilderlabs.com/products/ … c-filament

and click "MSDS".

5

Re: Extruding PVA?

elmoret wrote:

Where'd you see that avoid thermal decomposition? Here's the MSDS for Esun PVA:

https://cdn.shopify.com/s/files/1/0389/ … 4.pdf?7844

I have a writeup someone sent me on their PVA success, if you're interested I can upload it. As usual, a big key is pre drying the polymer.

I don't remember, I could be remembering incorrectly. Anyway, if you could upload that writeup, that would be awesome!

6

Re: Extruding PVA?

Should be attached.

Post's attachments

PVA extrusion-1.doc 2.31 mb, 28 downloads since 2015-09-18 

You don't have the permssions to download the attachments of this post.

7

Re: Extruding PVA?

Awesome, thank you so much!