Topic: Copper Infused Filament
Hello, I was wondering if there was any way to make copper infused filament without buying $50 pellets?
Thanks in advance.
James
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Filastruder → Copper Infused Filament
Hello, I was wondering if there was any way to make copper infused filament without buying $50 pellets?
Thanks in advance.
James
Sure, just add powdered copper to a base polymer.
The secret sauce is picking the right polymer, finding the right size powder, and figuring out the right mixing ratio.
SoliForum - 3D Printing Community → Filastruder → Copper Infused Filament
Powered by PunBB, supported by Informer Technologies, Inc.