1

Topic: LF Solidoodle .4mm nozzle

Hi im not sure were to post this but im looking for a same size .4mm nozzle, i dont want to order it from solidoodle website they are charging $45 to ship it and i cant find .4mm size anywere.

2

Re: LF Solidoodle .4mm nozzle

Elmoret is selling some old PEEK hotends in a B/S/T thread. See if he has any left and you can just rob it off the old ones.

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

3

Re: LF Solidoodle .4mm nozzle

http://www.soliforum.com/topic/12100/su … ks-tablet/