Topic: Filament Jam
I just got my duo a week ago and it has been nothing but problems. I keep getting the error extruder 2 jammed. I am using 2 new OEM cartridges. The extruder itself is not jammed. I swapped the two cartridges and same thing on extruder 2. Extruder 1 prints fine.
I will print for about 1 minute and it gives me the error. It will keep printing after the error for 20 seconds and then stop the print and the filament is coming out nicely with no clicking. I was watching the temperature and the extruder 2 never dropped below 209C.
The print bed only warms up to 70C instead of 90C and it warms up way faster than my AIO. In fact it warms up faster than the extruders and the leds dim while it is heating.
What does Da Vinci use to sense a fillament Jam?