1 (edited by keanu.m 2015-08-10 20:33:34)

Topic: Press doesn't want what i want

Hey Guys,
Maybe some of you had some strange prints like mine (photo) with the press?! any ideas what could be the reason for this
thanks already
greetz from germany

Post's attachments

IMG_3069.JPG
IMG_3069.JPG 3.2 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Press doesn't want what i want

Check the set screws for the pulley on the Y motor, mine were not even tapped through to the shaft.  Another example of bad quality control.

3

Re: Press doesn't want what i want

Whats the print speed ? Do you use retraction ?

Fat kids are harder to kidnap!