1

Topic: Printer Quality Problem - Please Help Me

Could someone help me with the problem below ???

Look at the difference between the same objects. Until last week all objects were printed perfectly, but now they are not solids and break easily.

I believed that I needed to calibrate the bed, but I did it and not solved.

Would anyone know how to solve?

Thank you.

Post's attachments

20150813_125531.jpg
20150813_125531.jpg 3.89 mb, 2 downloads since 2015-08-13 

20150813_125552.jpg
20150813_125552.jpg 4.04 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Printer Quality Problem - Please Help Me

You probably have a partially clogged nozzle/hotend.