Topic: How to deal with nozzle leaking problem?
If the nozzle happens to leak filament. It is because there is a gap between feeding tube and nozzle due to frequent nozzle disassembly
1 Remove the nozzle with the wrench in the tool box.
2 Wining one layer PTFE thread seal tape on the tube.
3 Screw the nozzle into the hot end tightly but gently.