1

Topic: Filament not sticking to platform, just goes into a blob

Hey so today when i try to print it seems that it dosent stick even when i use glue and my heated bed, im using repetier host on my da vinci and ive been using the printer for a month without problems.

2 (edited by carl_m1968 2015-07-27 03:56:25)

Re: Filament not sticking to platform, just goes into a blob

Use the manual bed leveling procedure at the top of this section in the forum. The bed has to be leveled on a two to four week average. It gets unlevel due to vibrations as well as you pulling parts from it.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Filament not sticking to platform, just goes into a blob

Your nozzle isn't close to the glass bed and your over extruding.