1 (edited by hansen644 2015-07-03 23:49:42)

Topic: Can not figure grinding problem out.

Pic attached.  Extruder gear keeps grinding filament ABS and PLA at all tempatures I have tried. Not sure what the problem is. Ideas?  Also prints have lots of pimples as seen in the pictures.  The grinding happens sometimes on the 3rd layer some times on the last few layers. No ryme or reason to when it starts to grind.  Note: using no fan with ABS and the printer is a smartone 200. I have tried slicer, cura, and simplied 3d.  all do the same thing.

Post's attachments

DSC00941.JPG 1.95 mb, file has never been downloaded. 

DSC00943.JPG
DSC00943.JPG 2.18 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Can not figure grinding problem out.

Check for these problems,  Low V-ref on extruder motor, Filament getting hanged up somewhere, partial clog on extruder.  I'm sure there are few others, but i'm not fully awake yet.. sorry wink

SD2 - Glass Bed, Fans on PCB and Y motor, Custom enclosure
Slicer - Simplify3D