Re: Da Vinci borosilicate glass with heater
rockosmodlife wrote:Regular glass has a linear thermal expansion coeff. of about 9x10^-6 m/m K
http://www.engineeringtoolbox.com/linea … -d_95.htmlAcrylonitrile Butadiene Styrene has a linear thermal expansion coeff. of about 73.8x10^-6 m/m K
http://www.engineeringtoolbox.com/linea … -d_95.htmlNot to mention that the glass is well below the hot-end temperature when printing ABS.
Doh! Good catch. I think the table I looked glass up on was expressed in 10^-7 and I didn't pay close enough attention. I guess I can toss that theory out the (plain) glass window!
![]()