<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Taulman 618]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/865/" />
	<updated>2013-05-06T13:44:20Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/865/taulman-618/</id>
		<entry>
			<title type="html"><![CDATA[Re: Taulman 618]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/21882/#p21882" />
			<content type="html"><![CDATA[<p>Theres a good extensive thread on both the Taulman 618 and a tiny bit on the new clear 645.</p><p><a href="http://www.soliforum.com/topic/466/nylon/">http://www.soliforum.com/topic/466/nylon/</a></p>]]></content>
			<author>
				<name><![CDATA[adrian]]></name>
				<uri>https://www.soliforum.com/user/663/</uri>
			</author>
			<updated>2013-05-06T13:44:20Z</updated>
			<id>https://www.soliforum.com/post/21882/#p21882</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Taulman 618]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/21870/#p21870" />
			<content type="html"><![CDATA[<p>Worked really great, oozed a bit more than I&#039;d like it to.&nbsp; The material was great though, but I didn&#039;t have a use for it on normal prints.&nbsp; I printed at about 205, with a fan on constantly.&nbsp; Printing at this temperature allowed the layers to adhere better to each other.</p>]]></content>
			<author>
				<name><![CDATA[aFoote]]></name>
				<uri>https://www.soliforum.com/user/319/</uri>
			</author>
			<updated>2013-05-06T06:02:36Z</updated>
			<id>https://www.soliforum.com/post/21870/#p21870</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Taulman 618]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/21865/#p21865" />
			<content type="html"><![CDATA[<p>So what did you guys find out? I&#039;m interested in trying this.</p>]]></content>
			<author>
				<name><![CDATA[emooney]]></name>
				<uri>https://www.soliforum.com/user/1109/</uri>
			</author>
			<updated>2013-05-06T02:30:02Z</updated>
			<id>https://www.soliforum.com/post/21865/#p21865</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Taulman 618]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/7742/#p7742" />
			<content type="html"><![CDATA[<p>Yeah I ordered mine, I&#039;m waiting on it to come though.&nbsp; </p><p>From what I can tell like ronsii said, our extruder when heated to 195 is equal to a higher temperature, so I&#039;ll give it a go heated at around 200 when I get it, and go from there. </p><p>I&#039;ll make sure to document and show pictures to everyone here when it comes in though!</p>]]></content>
			<author>
				<name><![CDATA[aFoote]]></name>
				<uri>https://www.soliforum.com/user/319/</uri>
			</author>
			<updated>2012-12-22T07:23:36Z</updated>
			<id>https://www.soliforum.com/post/7742/#p7742</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Taulman 618]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/7741/#p7741" />
			<content type="html"><![CDATA[<p>The extruder usually runs at least 30 degrees hotter then the setting you make in the control software.</p><p>I believe a few people on this forum are trying the taulman nylon.... aFoote I think is one of them????</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2012-12-22T06:45:51Z</updated>
			<id>https://www.soliforum.com/post/7741/#p7741</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Taulman 618]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/7740/#p7740" />
			<content type="html"><![CDATA[<p>Anybody tried this stuff?</p><p><a href="http://www.taulman3d.com/index.html">http://www.taulman3d.com/index.html</a></p><p>How can we turn the extruder up to the 240-250 needed?</p>]]></content>
			<author>
				<name><![CDATA[g00bd0g]]></name>
				<uri>https://www.soliforum.com/user/445/</uri>
			</author>
			<updated>2012-12-22T06:13:32Z</updated>
			<id>https://www.soliforum.com/post/7740/#p7740</id>
		</entry>
</feed>