<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — printing metal with a FDM - not a april fool joke anymore]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/6454/" />
	<updated>2014-08-04T09:51:18Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/6454/printing-metal-with-a-fdm-not-a-april-fool-joke-anymore/</id>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/61995/#p61995" />
			<content type="html"><![CDATA[<p>Nice filaments...good stuff indeed! I am also investigating to get some of these to my shop.</p>]]></content>
			<author>
				<name><![CDATA[oklok]]></name>
				<uri>https://www.soliforum.com/user/6232/</uri>
			</author>
			<updated>2014-08-04T09:51:18Z</updated>
			<id>https://www.soliforum.com/post/61995/#p61995</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/61692/#p61692" />
			<content type="html"><![CDATA[<p>NOTE: Apprently the Bronzefill is now mostly out of stock till the end of Aug. I&#039;ll have to make my roll last hehe</p><p>** I have been playing with this material and I LOVE it, especially since now I have the settings down- &gt; <a href="http://www.soliforum.com/topic/7012/colorfabb-bronzefill/">http://www.soliforum.com/topic/7012/col … ronzefill/</a></p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-08-01T13:03:14Z</updated>
			<id>https://www.soliforum.com/post/61692/#p61692</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60440/#p60440" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>LdyMox wrote:</cite><blockquote><p>muhahahaa..did this call for an evil laugh?</p></blockquote></div><p>Evil laughs are always welcome.&nbsp; <span class="postimg"><img src="http://www.thetruckersreport.com/truckingindustryforum/images/smilies/roundies/biggrin_25523.gif" alt="http://www.thetruckersreport.com/truckingindustryforum/images/smilies/roundies/biggrin_25523.gif" /></span></p><p><div class="fancy_video_tag_player"><iframe class="youtube-player" type="text/html" width="640" height="385" src="http://www.youtube.com/embed/PuY7BKNyKgM" frameborder="0"></iframe></div></p>]]></content>
			<author>
				<name><![CDATA[Downeasta]]></name>
				<uri>https://www.soliforum.com/user/2351/</uri>
			</author>
			<updated>2014-07-16T13:50:20Z</updated>
			<id>https://www.soliforum.com/post/60440/#p60440</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60438/#p60438" />
			<content type="html"><![CDATA[<p>It seems Printed Solid now added it to their products. <a href="http://www.printedsolid.com/shop/175-3/bronze/">http://www.printedsolid.com/shop/175-3/bronze/</a></p><p>I&#039;ll have some tomorrow in my hands and soon I can begin some testing (which I&#039;ll post results in the Filiment forum as I get them)...muhahahaa..did this call for an evil laugh? I don&#039;t know, but it seemed right somehow haha</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-07-16T13:25:00Z</updated>
			<id>https://www.soliforum.com/post/60438/#p60438</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60380/#p60380" />
			<content type="html"><![CDATA[<p><a href="http://www.printedsolid.com/">http://www.printedsolid.com/</a></p><p>*I brought some t-glase and the woodfill from them previously with no problems.</p><p>It is pricey stuff...but hopefully worth it.<br />750g spool was about $67<br />1.5kg spool was about $100</p><p>He don&#039;t have it one his site yet but taken from thier twitter AKA @PrintedSolid just yesterday...</p><p>&quot;Woohoo!&nbsp; limited amount of @colorfabb #bronzefill in stock for US shipments.&nbsp; DM or <a href="http://www.printedsolid.com/contact/">http://www.printedsolid.com/contact/</a>&nbsp; to order </p><p><span class="postimg"><img src="https://pbs.twimg.com/media/BshESfUCAAAc-UC.jpg" alt="https://pbs.twimg.com/media/BshESfUCAAAc-UC.jpg" /></span><br />&quot;</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-07-15T15:13:15Z</updated>
			<id>https://www.soliforum.com/post/60380/#p60380</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60379/#p60379" />
			<content type="html"><![CDATA[<p>Nice! Thanks for the link. The &quot;antique copper&quot; treatment looks snazzy. <br />Do you have a link for the US distributor?</p>]]></content>
			<author>
				<name><![CDATA[AZERATE]]></name>
				<uri>https://www.soliforum.com/user/4188/</uri>
			</author>
			<updated>2014-07-15T15:04:30Z</updated>
			<id>https://www.soliforum.com/post/60379/#p60379</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60377/#p60377" />
			<content type="html"><![CDATA[<p>Not long of a wait. It came out from Colorfabb about 2.5 weeks ago (in the Neatherlands). The US Distrbuter PrintedSolid took some orders last week and they mailed them out yesterday. I will probbaly get some in my hands on Thursday. </p><p>There is post processing needed to make it shine. I have heard people using sandpaper, dremmel tool, and/or rock polisher for the sanding; And for the polishing metal polish, ketchup etc. </p><p>Here is a quick How to print with Bronzefill link <a href="http://learn.colorfabb.com/print-bronzefill/">http://learn.colorfabb.com/print-bronzefill/</a><br />* I am gonna have to learn about antique patina and metals. That effect looks wicked.</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-07-15T14:45:11Z</updated>
			<id>https://www.soliforum.com/post/60377/#p60377</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60375/#p60375" />
			<content type="html"><![CDATA[<p>I&#039;m totally looking forward to your results...if it&#039;s as good as advertised, I&#039;m gonna pick up a spool.<br />How long has the wait been for you to get it (so far)?</p>]]></content>
			<author>
				<name><![CDATA[AZERATE]]></name>
				<uri>https://www.soliforum.com/user/4188/</uri>
			</author>
			<updated>2014-07-15T14:33:54Z</updated>
			<id>https://www.soliforum.com/post/60375/#p60375</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60369/#p60369" />
			<content type="html"><![CDATA[<p>I&#039;m quite excited. I should have some of this stuff by the end of the week!</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-07-15T12:24:23Z</updated>
			<id>https://www.soliforum.com/post/60369/#p60369</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/60014/#p60014" />
			<content type="html"><![CDATA[<p>This Color fab bronzefill is out now for it&#039;s beta run. I will be getting some from PrintedSolid(a US reseller of colorfabb) once they get some in a few weeks. This stuff is 80% bronze powder/20% PLA and something like 3 to 4 times heavier then PLA. </p><p>There is stuff on twitter about it including some sample prints. I can&#039;t wait to get my hands on this stuff!</p><p><a href="https://twitter.com/hashtag/bronzefill">https://twitter.com/hashtag/bronzefill</a></p><p><a href="http://colorfabb.com/bronzefill#.U72dMNgo9D8">http://colorfabb.com/bronzefill#.U72dMNgo9D8</a></p><p>Once I have it in my hands...I&#039;ll do some testing</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-07-09T19:35:05Z</updated>
			<id>https://www.soliforum.com/post/60014/#p60014</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/57915/#p57915" />
			<content type="html"><![CDATA[<p>I&#039;ll buy a spool once I start an off shore bank account to sneak it past the wife</p>]]></content>
			<author>
				<name><![CDATA[AZERATE]]></name>
				<uri>https://www.soliforum.com/user/4188/</uri>
			</author>
			<updated>2014-06-04T16:59:14Z</updated>
			<id>https://www.soliforum.com/post/57915/#p57915</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/57911/#p57911" />
			<content type="html"><![CDATA[<p>You can preorder the bronzeFill now <a href="http://colorfabb.com/bronzefill#.U49L29go9D8">http://colorfabb.com/bronzefill#.U49L29go9D8</a></p><p>So tempting except I&#039;m in the states and the shipping is quite pricey. I might do it anyways even if a spool ends up costs waaay too much. </p><p>Clearly the benefit of this is getting a bronze look, the drawback is that you need to polish it and thus will likely lose much detail.</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-06-04T16:46:05Z</updated>
			<id>https://www.soliforum.com/post/57911/#p57911</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/56697/#p56697" />
			<content type="html"><![CDATA[<p>Wonder what special new things you can print in bronze.....</p>]]></content>
			<author>
				<name><![CDATA[Ggalisky]]></name>
				<uri>https://www.soliforum.com/user/5970/</uri>
			</author>
			<updated>2014-05-21T03:11:43Z</updated>
			<id>https://www.soliforum.com/post/56697/#p56697</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/56686/#p56686" />
			<content type="html"><![CDATA[<p>Very excited by that bronze one, especially when polished. Thanks for the link.</p>]]></content>
			<author>
				<name><![CDATA[lawsy]]></name>
				<uri>https://www.soliforum.com/user/51/</uri>
			</author>
			<updated>2014-05-20T22:24:06Z</updated>
			<id>https://www.soliforum.com/post/56686/#p56686</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing metal with a FDM - not a april fool joke anymore]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/56632/#p56632" />
			<content type="html"><![CDATA[<p>Want the bronze fill...must have...</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-05-20T13:14:34Z</updated>
			<id>https://www.soliforum.com/post/56632/#p56632</id>
		</entry>