<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — SD4 horizontal stripes on prints]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/11042/" />
	<updated>2015-05-17T00:42:16Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/11042/sd4-horizontal-stripes-on-prints/</id>
		<entry>
			<title type="html"><![CDATA[Re: SD4 horizontal stripes on prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96050/#p96050" />
			<content type="html"><![CDATA[<p>do a bit of digging around - there are plenty of threads about it. </p><p>I personally have not needed to do that to my SD4, so I cant really tell ya much. I was able to solve what little banding I had with a simple bed stabilizer on the front.</p>]]></content>
			<author>
				<name><![CDATA[heartless]]></name>
				<uri>https://www.soliforum.com/user/10399/</uri>
			</author>
			<updated>2015-05-17T00:42:16Z</updated>
			<id>https://www.soliforum.com/post/96050/#p96050</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: SD4 horizontal stripes on prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96037/#p96037" />
			<content type="html"><![CDATA[<p>Thanks. This helped me a bit.<br />I&#039;ve read a couple of fellow SD owners changed their 5/16 threaded rods to M3 threaded rods, but haven&#039;t found any details. Is there anybody who could tell me how should I do it?</p>]]></content>
			<author>
				<name><![CDATA[mdonci]]></name>
				<uri>https://www.soliforum.com/user/9233/</uri>
			</author>
			<updated>2015-05-16T22:12:34Z</updated>
			<id>https://www.soliforum.com/post/96037/#p96037</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: SD4 horizontal stripes on prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/95179/#p95179" />
			<content type="html"><![CDATA[<p>That is a mechanical problem commonly referred to as Z wobble. it has nothing to do with the type of filament. </p><p>there is a lot of discussion about it and various ways of trying to fix it - there is a stickied thread just above about this very subject. <a href="http://www.soliforum.com/topic/2154/fixing-banding-zwobble-with-fine-threaded-zrod/">http://www.soliforum.com/topic/2154/fix … aded-zrod/</a></p>]]></content>
			<author>
				<name><![CDATA[heartless]]></name>
				<uri>https://www.soliforum.com/user/10399/</uri>
			</author>
			<updated>2015-05-08T12:02:26Z</updated>
			<id>https://www.soliforum.com/post/95179/#p95179</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[SD4 horizontal stripes on prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/95176/#p95176" />
			<content type="html"><![CDATA[<p>Hi,</p><p>I have a big problem with my SD4. When I print, horizontal stripes appear on my prints. I&#039;ve tested cheap Chinese filament and an expensive premium EU filament. What could be the problem? <br />See the images below</p>]]></content>
			<author>
				<name><![CDATA[mdonci]]></name>
				<uri>https://www.soliforum.com/user/9233/</uri>
			</author>
			<updated>2015-05-08T10:21:32Z</updated>
			<id>https://www.soliforum.com/post/95176/#p95176</id>
		</entry>