I'm getting long strands of plastic stuck to the sides of things anytime the head has to travel with no infill.  I thought the extruder was too hot, but I'm down to 195 (abs) and it's still happening.  I did the firmware correction from "solidoodletips.wordpress" (not allowed to post URLs yet!), and turned it down by about 30%.  But it's still happening. 

Any suggestions?  I'm mostly using the .3mm slicr settings from solidoodle, although I've slowed the perimeter speed down to 30 to make circles come out better.

Picture is attached, because no links. smile

Post's attachments

8366599632_4933991b37_z.jpg
8366599632_4933991b37_z.jpg 223.96 kb, 2 downloads since 2013-01-10 

You don't have the permssions to download the attachments of this post.

2

Re: What am I doing wrong? (slicr)

Start with retraction settings in Slic3r, make the number higher.