Hello,

I have some Cyrolite Hiflo Acryllic that I would like to use for filament in my Davinci 3D

In the filastruder set at temp of 205 C it extrudes fine. However, in the Davinci set between 210-230 C extrusion temp I have trouble to get the first layer to stick (bed temp at 90 C)

Should I increase the bed temp ?

ABS has no issue, I use a first layer of hair spray and then some glue on top.

Did anyone use acrylic successfully ?

2

Re: Cyrolite HiFlo Acryllic ?

Setting the extruder on the Davinci to 250 C did the trick. Print sticking well to bed and coming out great.