Topic: PLA - BASF Ecovio C2224
Hello everyone!
Have you guys tried the Ecovio C224 from Basf? I have just tried but it seems to be too soft.
Tim, do you know this material?
Here's its datasheet:
http://www.plasticsportal.net/wa/plasti … _C2224.pdf
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Filastruder → PLA - BASF Ecovio C2224
Hello everyone!
Have you guys tried the Ecovio C224 from Basf? I have just tried but it seems to be too soft.
Tim, do you know this material?
Here's its datasheet:
http://www.plasticsportal.net/wa/plasti … _C2224.pdf
The only PLA I've ever used was 4043D. Extruded at 155C or so, needs good cooling and needs to be predryed well.
Note that what you linked is a blend, only 45% PLA.
SoliForum - 3D Printing Community → Filastruder → PLA - BASF Ecovio C2224