1

Topic: Kinds of ABS

Hello!

Have you guys ever tried any of the following ABS pallets?

ABS NATURAL BASF GP 35
ABS NATURAL BASF GP 35
ABS NATURAL BASF GP 35
ABS NATURAL CHEIL MP 0160R
ABS NATURAL CHEIL SD 0170W
ABS NATURAL CHEIL SV-0167
ABS NATURAL EM PO KUMHO HR 181
ABS NATURAL FORMOSA AE8000
ABS NATURAL FORMOSA AE8000
ABS NATURAL KUMHO 750SW
ABS NATURAL KUMHO 750SW
ABS BLACK CHEIL SD 0150 / K2007
ABS BLACK CHEIL SD 0150 / K23212
ABS BLACK V0 HFA 451 KUMHO
ABS TRANSPARENT TERLUX 2802 TR

Thanks!

2

Re: Kinds of ABS

Hi, I personally haven't tested any of those, but as general rule you have to look for virgin material, for thin-wall applications (moulding, not extrusion) and with high Melt Flow rate.

3

Re: Kinds of ABS

GP35 should be fine - its even higher MFI than GP22 which OS Printing used to sell/use. GP22 extruded at about half the speed of MG94, so GP35 should be fine.