Hi all!

I was inspired by Ian and Josh about smoothing the prints with acetone.
I found an egg cooker and tried some small prints - and it was great! The size is a limit, but my overall prints isn't filling the whole space inside the cooker afterall.

Here is a quick overview of the little process:
http://sphotos-g.ak.fbcdn.net/hphotos-ak-ash3/617134_10152242161995106_1353708703_o.jpg

Close up - Sanded down:
http://sphotos-h.ak.fbcdn.net/hphotos-ak-ash3/617090_10152242161905106_1566489915_o.jpg

A small amount of acetone - pour into the futuristic machine:
http://sphotos-h.ak.fbcdn.net/hphotos-ak-ash3/525520_10152242162070106_122702491_n.jpg

Turn on the egg cooker and wait for 20 seconds:
http://sphotos-c.ak.fbcdn.net/hphotos-ak-ash4/665913_10152242162135106_166959505_o.jpg

The finished product. I could have put more time in sanding, but first test anyways big_smile
http://sphotos-g.ak.fbcdn.net/hphotos-ak-ash4/664384_10152242161830106_1559236910_o.jpg

Solidoodle 2 - Repetier Host V0.82 - Slic3r 0.9.7

2

Re: Smoothing station - Egg cooker

Nice writeup! Can't wait to get my printer to test something similar out.

[Hyggelig å se en annen nordmann på forumet  smile ]

3

Re: Smoothing station - Egg cooker

Hmm cool smile Might try the same myself.. big_smile

[Nordmenn er vi nok av her big_smile]

4 (edited by RSandven 2012-11-11 15:48:39)

Re: Smoothing station - Egg cooker

I will try some more soon. The concept seems very easy.
But it seems that my Z-axis is a bit wobbly.
(Hyggelig med nordmenn ja big_smile)

Solidoodle 2 - Repetier Host V0.82 - Slic3r 0.9.7

5

Re: Smoothing station - Egg cooker

This will be tried!

[Hei på dere big_smile]

6

Re: Smoothing station - Egg cooker

Wow! It's great! I managed to find the exactly same cooker (12 euros) and it's working like a charm! Thanks!

7

Re: Smoothing station - Egg cooker

how big of objects could this smooth? what are dimensions

8

Re: Smoothing station - Egg cooker

newto3dprinting1 wrote:

how big of objects could this smooth? what are dimensions

At least egg sized objects will fit. tongue

No trees were harmed in the creation of this email, though some electrons were horribly inconvenienced.

9

Re: Smoothing station - Egg cooker

Agree,hehe

iowajames wrote:
newto3dprinting1 wrote:

how big of objects could this smooth? what are dimensions

At least egg sized objects will fit. tongue