1

Topic: Very Recent Extrusion

Finally had a little free time to run off some more ABS filament last night and run off a test print tonight. Was going for extremely rapid color changes in print... decent results sadly the camera phone does it no justice. Straight vertical extrusion from about 5 feet in the air, self coiling on floor then wound onto spool. Second Filament is still running, doing a very slow fade from red to yellow to blue then back to red, then running the rest of the spool out as white. http://r3screations.com/1.jpghttp://r3screations.com/2.jpghttp://r3screations.com/3.jpg

2

Re: Very Recent Extrusion

Wow - that vase looks great! Rotated:

http://i.imgur.com/5wxNysv.jpg?1