1

Topic: Jesse's Filastruder Build

Some photos of my Filastruder kit.  I haven't successfully printed out the electronics v2 case.  ABS warps too much and PLA got clogged in the nozzle.  I may just make it out wood.

Post's attachments

aa8c84c137929d910bebaa9062f4225c.JPG
aa8c84c137929d910bebaa9062f4225c.JPG 2.53 mb, 1 downloads since 2013-05-31 

Qc1JDGmh.jpg
Qc1JDGmh.jpg 112.42 kb, file has never been downloaded. 

z7L7jLFh.jpg
z7L7jLFh.jpg 123.61 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Jesse's Filastruder Build

Cool!

This might be easier to print:
http://www.thingiverse.com/thing:94429

3

Re: Jesse's Filastruder Build

Thanks Tim!  I probably spent 8 hours total trying to print that case.

Simplicity FTW

4

Re: Jesse's Filastruder Build

jesse wrote:

Thanks Tim!  I probably spent 8 hours total trying to print that case.

:-/ Sorry. it worked okay on my enclosed Solidoodle but I didn't think about non-enclosed printers.

Sweet looking filament! Can you comment more on how you made it?

5

Re: Jesse's Filastruder Build

elmoret wrote:

Sweet looking filament! Can you comment more on how you made it?

I made layers in the hopper 1 to 2 cm thick.  A layer consisted of white ABS pellets mixed with one colorant.  Eventually all the layers get gradually mixed together as the stack falls into the middle.

I just finished printing a hollow calibration pyramid from filastruder-made filament.  The white ABS pellets came from eBay user "carlsievering".  Not a bad result.  The filament was supposed to be red but turned out pink.  Not sure why.

Post's attachments

IMG_4740.JPG
IMG_4740.JPG 1.99 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

6

Re: Jesse's Filastruder Build

Nice!

Pink means either not enough colorant, or you have white ABS (which already has white colorant in it). Did you buy white or natural? Link?

Incidentally most of Carl's stuff is Sabic MG94, which is great for 3D printing. There are rumors that it's what Stratasys uses. It's what OS Printing sells and what I include with Filastruders.

7

Re: Jesse's Filastruder Build

What kind of delta bot is that?  It almost looks like you are printing on a record.

8

Re: Jesse's Filastruder Build

Also, if it's not too much trouble could yo use www.imgur.com so your pictures are inline?

9 (edited by jesse 2013-06-01 02:29:39)

Re: Jesse's Filastruder Build

The printer is a Rostock Max.  I think the reason why the filament came out pink is because the ABS pellets from Carl's eBay store have white pigment unlike the OSP LLC. pellets.

http://www.makexyz.com/printer/jesse

elmoret wrote:

Also, if it's not too much trouble could yo use www.imgur.com so your pictures are inline?

http://i.imgur.com/cxQOYmB.jpg
http://i.imgur.com/CjrsH33.jpg
http://i.imgur.com/77elMZe.jpg
http://i.imgur.com/92UDEG1.jpg

10

Re: Jesse's Filastruder Build

"  I think the reason why the filament came out pink is because the ABS pellets from Carl's eBay store have white pigment unlike the OSP LLC. pellets."

He might be out of the natural, but I got 18 lbs of it from him in addition to ten pounds of white.

11

Re: Jesse's Filastruder Build

Nimikin wrote:

He might be out of the natural, but I got 18 lbs of it from him in addition to ten pounds of white.

Yes, I messaged him and he said he ran out of natural.  Be aware that white pellets don't really color that well.

12

Re: Jesse's Filastruder Build

Printed the electronics plate, removed aluminum foil, added kapkon tape.

http://i.imgur.com/3IN7EO6.jpg
http://i.imgur.com/lVlhH6H.jpg
http://i.imgur.com/DJiUko3.jpg

13

Re: Jesse's Filastruder Build

elmoret wrote:

Incidentally most of Carl's stuff is Sabic MG94, which is great for 3D printing.

Just curious, how do you know that most of Carl's stuff is Sabic MG94?

14

Re: Jesse's Filastruder Build

jibberjive wrote:
elmoret wrote:

Incidentally most of Carl's stuff is Sabic MG94, which is great for 3D printing.

Just curious, how do you know that most of Carl's stuff is Sabic MG94?

It was in the auction description.

15

Re: Jesse's Filastruder Build

Ah, didn't see that.

16

Re: Jesse's Filastruder Build

Did some filament making today, probably about 1 pound over about 5-6 hours.

http://i.imgur.com/leVLnWA.jpg
http://i.imgur.com/opN0mRG.jpg
http://i.imgur.com/aUR36ra.jpg
http://i.imgur.com/XvY0hxy.jpg

17

Re: Jesse's Filastruder Build

I made a spool and used an electric drill to wind it up.

http://i.imgur.com/cxRTahE.jpg
http://i.imgur.com/wIMGRRW.jpg
http://i.imgur.com/tgYPhoP.jpg

18

Re: Jesse's Filastruder Build

Have you tried printing anything with your rainbow filament Jesse?
I wonder what it would look like...