Hello, please advise a not brittle (or less than usual brittle) resin. Red good reviews on Siraya resin, but there is no stock in the UK, any alternatives?
This is for a small batch production of protective caps.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → SLA Printers → non brittle resin
Hello, please advise a not brittle (or less than usual brittle) resin. Red good reviews on Siraya resin, but there is no stock in the UK, any alternatives?
This is for a small batch production of protective caps.
Hello, please advise a not brittle (or less than usual brittle) resin. Red good reviews on Siraya resin, but there is no stock in the UK, any alternatives?
This is for a small batch production of protective caps.
Try searching for ABS - Like Resin. it's about as good as you will get unless you want to get the tough resin which is very expensive.
Vlad wrote:Hello, please advise a not brittle (or less than usual brittle) resin. Red good reviews on Siraya resin, but there is no stock in the UK, any alternatives?
This is for a small batch production of protective caps.Try searching for ABS - Like Resin. it's about as good as you will get unless you want to get the tough resin which is very expensive.
Have you used this resin before Carl? If yes, what did you think?
carl_m1968 wrote:Vlad wrote:Hello, please advise a not brittle (or less than usual brittle) resin. Red good reviews on Siraya resin, but there is no stock in the UK, any alternatives?
This is for a small batch production of protective caps.Try searching for ABS - Like Resin. it's about as good as you will get unless you want to get the tough resin which is very expensive.
Have you used this resin before Carl? If yes, what did you think?
I use it now. It is slightly more flexible than normal resins. Ilt is not as prone to chipping or breaking if dropped. It is still not as durable as FDM printed materials.
You need this one: https://ameralabs.com/shop/tgm-7-led/