Topic: New hot end for Da Vinci Super any one?

Hello everyone
I have access to a da vinci super put the whole assembly of the hot end is unreliable and it clogs very easy. Has anyone tried to modify the cartridge we with a more reliable hot end ?

2

Re: New hot end for Da Vinci Super any one?

What the heck is a Da Vinci Super and do you own the only one in existence?

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: New hot end for Da Vinci Super any one?

https://www.xyzprinting.com/en-US/produ … inci-super

4

Re: New hot end for Da Vinci Super any one?


You may just be the only owner of one. So you may be the pioneer for all the addons.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

5

Re: New hot end for Da Vinci Super any one?

One thing to try is using a different cooling fan on the heat sink; one with higher CFM to try end eliminate any heat creep which might be the root cause of the jamming.