1

Topic: SABIC MG47F ?

I would like to know whether SABIC MG47F ABS works for extrusion and 3D printing as MG94 ?

comparison here :

https://www.sabic.com/en/products/compa … 0c2926daac

min Qt to buy is 25kg that's why i'm asking before buying.

2

Re: SABIC MG47F ?

Forum search "MG47" = no cat in the horizon

google search http://www.soliforum.com/topic/14945/abs-mg47-cycolac/

3

Re: SABIC MG47F ?

Melt flow is lower so it would extrude slower, but it should still be usable for filament extrusion.  I can’t guarantee it since I haven’t used this specific type, but in general ABS is the easiest to extrude.