Topic: Filament storage question

most of the time I only have 2 to 3 spare rolls of filament.
I am thinking of using a 5 Gallon bucket with a screw on lid. put a piece of PVC pipe in the middle to drop the spools on with this Dehumidifying rod inside the pipe. would it dry the filament out to much.

Thanks
Dale
http://soliforum.com/i/?DE4zGof.jpg

https://www.amazon.com/SnapSafe-Inches- … amp;sr=8-5

Ultimaker S3.

2

Re: Filament storage question

dubbsd wrote:

most of the time I only have 2 to 3 spare rolls of filament.
I am thinking of using a 5 Gallon bucket with a screw on lid. put a piece of PVC pipe in the middle to drop the spools on with this Dehumidifying rod inside the pipe. would it dry the filament out to much.

Thanks
Dale
http://soliforum.com/i/?DE4zGof.jpg

https://www.amazon.com/SnapSafe-Inches- … amp;sr=8-5

Might want to read the reviews on that, and see the pictures on the broken plug. looks like a fire hazard to me. Just get a desiccant or silica gel and keep in the bucket as well.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Filament storage question

There are reusable desiccants you can dry out in the oven.