Topic: 3D printed retro car Hotrod Pickup that was made as a gift.

Hi folks!

I just want to share my new work! I made this car as a gift to my grandfather. He is a real fan of retro car, especially Hotrod.

Highlights:
Printer Tronxy x3, HC19-carbon plastic, nozzle 0.4.
The height of the compressor layer, unit, valve covers, headlights, grille is 0.15, and the rest is 0.3.
Nozzle temperature is 230 C.
Table — 80 C.
Blowing minimum.

Free STL: https://www.thingiverse.com/thing:2465732

https://reprap.org/forum/thumbcache/02c/332/cbd/0f0/a60/06f/37d/6d3/087/ff7/30_800x400.png

https://reprap.org/forum/thumbcache/5a7/682/f92/c4d/8ab/a92/76f/cdd/e53/d94/6d_800x400.png

https://reprap.org/forum/thumbcache/31b/a7b/b80/06f/8ac/a36/9e0/f59/8f9/d45/e1_800x400.png

https://reprap.org/forum/thumbcache/34c/4cd/25f/ec7/a18/aa6/509/eef/ae2/869/f5_800x400.png

https://reprap.org/forum/thumbcache/9a9/bbb/d58/081/987/cd7/235/751/c1e/1c8/f9_800x400.png

Process:

https://reprap.org/forum/thumbcache/602/3ac/47e/cfe/884/36e/ee0/c3e/06d/738/1b_800x400.png

https://reprap.org/forum/thumbcache/f2b/180/043/b55/308/b19/6b1/339/cd3/89c/0c_800x400.png