1

Topic: Problems with plastic extruder upgrade breaking.

The part where the PTFE tubing slides into the extruder is breaking this is my 3rd set in a year
I have also had a lot of trouble with the tubing coming out of the top of the extruder.
I am wondering if i can adapt this to it. and if they would work.
http://soliforum.com/i/?8hpMQat.jpg


Here id the fitting I want to adapt.
http://soliforum.com/i/?yaxpE6L.jpg

https://www.amazon.com/dp/B07CCN99FB/re … 18503a9aad

Ultimaker S3.

2

Re: Problems with plastic extruder upgrade breaking.

You really don't need the tubing unless you are using the spool holders on the back machine. To me it looks like the tubing movement is being restricted most likely by your cover not allowing enough movement. I would make small holes in the top of the cover and feed filament from over head without the tubes.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Problems with plastic extruder upgrade breaking.

Thanks Carl

Ultimaker S3.

4

Re: Problems with plastic extruder upgrade breaking.

you are missing this

https://www.thingiverse.com/thing:200182

The bowden tube ID is too small, will increase resistance for filament feeding. The ID is only slightly bigger than you filament, will be good for bowden setup after extruder motor, not good for direct drive before extruder motor.

There is many extruder upper arm that have stronger PTFE tubing holder.

https://www.thingiverse.com/thing:222667

(Da Vinci 1.0, Jr. 1.0 RAMPS, miniMaker) X4, (Creality CR-10S, CR-10 mini, Ender-3) X4, Anycubic MEGA X4, Anycubic Chrion X1, ADMILAB Gantry X2 (MonoPrice Maker Select V2, Plus, Ultimate)X4--Select mini X1, Anycubic photon X4, Wanhao duplicate D7 X1.
iNSTONE Inventor Pro X2, CTC Dual X2, ANET-A8, Hictop 3DP-11, Solidoodle Press, FLSUN I3 2017X1

5

Re: Problems with plastic extruder upgrade breaking.

I have the upgraded extruder parts and the Tubing holder. and they still broke.

Ultimaker S3.