1

Topic: Polycast or any low melting temperature point resin

Hello guys! How are you?

Do you guys know which resin is Polycast made of? I'm looking for a low melting temperature resin to extrude. Any thoughts about it?

Thank you!

Best Regards,
Rick

2 (edited by Tin Falcon 2018-01-28 14:54:37)

Re: Polycast or any low melting temperature point resin

http://www.machinablewax.com/product.php?product=52
Wax but keep in mind you must disable your cold extrude on your printer to use this.
The other option is to contact machinable wax and see if they will sell  you that blend in bulk.

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura