Yesterday I tried a black ABS 1.75mm filament (I had white before) and for some reason the filament is coming out really thin (0.24-0.33mm). Also, beside the main filament that's coming out, a tiny and very thin shaving is coming out (almost like there is a very tiny hole beside the main extrusion hole).

What's causing this? Is it a clogged extruder head? What's the best way to clean it? Can I take it off so may be I can clean it properly outside of the extruder assembly.

Thank you!

2

Re: SD3 very thin filament extrusion

did you calibrate your extrusion multiplier for that roll of filament?

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

3

Re: SD3 very thin filament extrusion

Not yet, will do it tonight smile

4

Re: SD3 very thin filament extrusion

Check that your nozzle isn't partially clogged.