Topic: Inconsistent filament print
Have solidoodle 4 and this is first time it's done this. Left side of print is fine right side no filament. See pic below. Using rept host and spic3r.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → Inconsistent filament print
Have solidoodle 4 and this is first time it's done this. Left side of print is fine right side no filament. See pic below. Using rept host and spic3r.
Need to level your bed.
I'll do that. Thanks!
and looking at those x axis rods, think its about time for news ones. look all scratched up
oh my... definitely need some new rods...