I've been printing in bronzefill on and off and I want to start using SS, CF, and some other exotic PLA mixes and was wondering if anyone had some feedback about if a hardened nozzle has helped with wear. My stock e3dlite6 nozzle isn't worn or anything, but just wondering if the price is worth it vs just buying a few spare brass ones, especially since I want to start running these filaments more regularly.

Thanks!

FuseBox 1.5 CoreXY - e3dv6 - Graphic Smart Display
Solidoodle 2 - e3dv6 - Hobb Goblin - e3d Titan - lawsy carriages - Direct Drive Y Axis - T8 Z axis - OctoPi

2

Re: hardened nozzles

Brass nozzles wear about 20 times faster than hardened. If you plan to print more than a few hundred grams of those materials, a hardened nozzle makes sense.