I posted a topic here a little while back on Encom 2012 PC, but I'm out and there isn't any more of that resin available on ebay.

What do you guys think of this? LEXAN 500-739 https://www.sabic-ip.com/gepapp/eng/wea … ype=Online

Melt flow rate: 7.5 g/10min

(Melt flow is a LOT lower than the encom, but I think this is good because I had a really bad problem with it stretching when it exits the nozzle. I had to make special modifications to the filastruder to allow it to cool before leaving the nozzle. The Encom 2012 was considered "high flow" at 20 g/10min)

-Prusa i3 MK2s
-Airwolf HD2x w/ E3D v6 + Volcano
-Custom built Solidoodle 3 clone w/ E3D v6+ Volcano    -Solidoodle Press w/ E3D Lite6