Topic: shaxon filament

I just ordered a cartridge resetter from Wctek the pro version it was only 5 bucks more hope this is a good unit to work with my 1.0,
I am going to frys today they have the shaxon filament is this ok to use in my 1.0 with the above resetter.

Thanks

2

Re: shaxon filament

jamerfut wrote:

I just ordered a cartridge resetter from Wctek the pro version it was only 5 bucks more hope this is a good unit to work with my 1.0,
I am going to frys today they have the shaxon filament is this ok to use in my 1.0 with the above resetter.

Thanks

Only use their basic colors like red, black, blue, and natural. Their bright and neon colors have proven near impossible to get to print correctly.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: shaxon filament

Thanks Carl_m1968 that's exactly what i bought today i will give it a try.