Topic: 3d print part crack line start to show up after acetone bath a week

Hi,

Hope I got the right forum.

Crack line start to show up after a week on my 3d printed part with acetone bath treatment, have anyone encounter this before? I spend hour of making the parts look smooth and shiny with acetone bath but crack line start appearing at the layer joins after a week. I am thinking because the abs contracts when it dry from the acetone bath. Any idea or fixes?

Thanks

2 (edited by n2ri 2014-08-23 00:54:13)

Re: 3d print part crack line start to show up after acetone bath a week

vapor or liquid? ABS absorbs liquids and acetone dont wash out with water etc. or need thicker walls or closer layer settings if vapor done it

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

3

Re: 3d print part crack line start to show up after acetone bath a week

Try sticking the parts in the freezer for several hours. That stops parts warping when they've had acetone soaked into them to strengthen the part, so it may well help here too.