Topic: NinjaFlex?
Anyone tried using NinjaFlex with the Da vinci?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → NinjaFlex?
Anyone tried using NinjaFlex with the Da vinci?
Yes, and it don't work.
It needs a similar mod to the replicators and makerbots to make it work.
I tried without and the filament eventually works its way out the side of the extruder head.
It hangs out there and mocks you.