Printed a Muskie lure off thingaverse and was wondering about the type
Paint and finish to use. I will be air brushing the lure. Thanks
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Projects → Paint /finish
Printed a Muskie lure off thingaverse and was wondering about the type
Paint and finish to use. I will be air brushing the lure. Thanks
I have used this (it will not melt the ABS.)
http://www.testors.com/category/133656/
Any acrylic based paint should work well on ABS