I have the 1-pound bag of Santoprene from the Filastruder store waiting for me to extrude, wondering if anyone has any pointers before I use it, specifically extrusion temperature, nozzle size (OEM or enlarged) and filament cooling.

2 (edited by BFeely 2021-11-10 20:59:17)

Re: Parameters for Santoprene 80A from Filastruder store

My results so far, 183C, OEM nozzle size, getting 1.63mm filament, and the Filastruder is extruding FAST - i.e. the winder can hardly keep up.