1

Topic: Set PID

Dear, I am from Chile and I have bought the Filastruder for a year and I still cannot operate it, from its assembly, which is very complicated, to its configuration. I'm disappointed.
I need to be told step by step to set the PID to 185 ° or any other temperature.
The post-sale service is terrible since the person who attends it does not respond adequately.
Help me set the PID

Ricardo

2

Re: Set PID

Sounds like this project is above your technical skill. The instructions are more than adequate to get the machine running, I have built several. There is no "Set X & Y to these values" and you're done. You have to experiment a little to figure the best settings for your own particular setup. IF you would like some personal help send me a PM. My fees are reasonable.

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

3 (edited by erosion139 2021-05-24 00:58:22)

Re: Set PID

rerazo55 wrote:

Dear, I am from Chile and I have bought the Filastruder for a year and I still cannot operate it, from its assembly, which is very complicated, to its configuration. I'm disappointed.
I need to be told step by step to set the PID to 185 ° or any other temperature.
The post-sale service is terrible since the person who attends it does not respond adequately.
Help me set the PID

Ricardo


1: press either the up arrow or down arrow. This will make the decimal point start to blink.
2: press the left pointing arrow button to select which digit is to be changed. EX: 000.0 00.00 0.000
3: press either the up or down arrows again while in this decimal flash mode to raise or lower the digit selected.
4: press SET, it will show a number like (A100).
5: press SET again until you see the green number read the temperature you desire. The decimal will no longer blink and the red temperature will gradually approach the green value.