hi there,

i was wondering if it would be possible to make plastic pellets by melting them in a pot and having it drip out through a nozzle into a bucket of water like how lead BBs are made as oppose to using a shredder.

2

Re: making plastic pellets

do not think it is that simple.
look here
http://www.homemadepelletmill.com/blog/ … llets.html

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura

3

Re: making plastic pellets

most plastics have a life to them. they can only be heated cycle so many times before it starts to break down. You would be better off with a shredder

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28